Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Discoloration Transformation Cream - Happi
Skin Care

Discoloration Transformation Cream

Coast Southwest created a new idea in skincare.

Released By Coast Southwest, Inc.

Discoloration Transformation Cream
Beauty Agent Studio/Shutterstock.com
Ingredients
%

Phase A

  • Deionized Water (Water)
  • 77.90
  • Propylene Glycol USP (Coast Southwest, Inc.) (Propylene Glycol)
  • 1.50
  • 3V Allantoin (Coast Southwest, Inc., 3V Sigma USA) (Allantoin)
  • 0.35
  • Endicare SC-530 (Coast Southwest, Inc.) (Polyethyloxazoline)
  • 1.00

Phase B

  • Lilac (Coast Southwest, Inc., Sonneborn LLC) (C14-C22 Alkane)
  • 5.00
  • Sensoderm DCE (Coast Southwest, Inc., 3V Sigma USA) (Dicaprylyl Ether)
  • 3.00
  • C'Ester MM (Coast Southwest, Inc., Ethox Chemicals, LLC) (Myristyl Myristate)
  • 1.50
  • Ethoxcare 4895 (Coast Southwest, Inc., Ethox Chemicals, LLC) (Cetearyl Alcohol (and) Steareth-30 (and) Ceteth-10)
  • 2.75

Phase C

  • Endiguard CAP-5 (Coast Southwest, Inc.) (Phenoxyethanol (and) Caprylyl Glycol (and) Potassium Sorbate (and) Hexylene Glycol)
  • 1.00
  • EndiMoist HA Solution (Coast Southwest, Inc.) (Sodium Hyaluronate)
  • 2.00
  • Endicare ETP-500 (Coast Southwest, Inc.) (Sodium Acrylate/Sodium Acryloyldimethyl
  • 2.00
  • OA Maslinox C (Coast Southwest, Inc., EG Active Cosmetics) (Water (and) Polycaprolactone (and) Ascorbyl Palmitate (and) Olea Europaea (Olive) Fruit Extract (and) Maslinic Acid (and) Hydroxytyrosol (and) Polyvinyl Alcohol (and) Caprylic/Capric Triglyceride (and) Sorbitan Stearate (and) Potassium Sorbate (and) Sodium Benzoate (and) Sodium Phytate (and) Xanthan Gum)
  • 2.00

Procedure

Phase A - Combine Phase A in main vessel with moderate mixing until uniform and clear. Begin heating to 55°C to 60°C. Phase B - In a side vessel, combine Phase B. Heat to 55°C to 60°C or as needed to melt Phase B completely. At temperature, slowly add Phase B to Phase A with increased mixing speed as needed. Discontinue heat. Phase C - Below 40°C, add Phase C ingredients in formula order with moderate mixing. Cool completely.

Properties

pH: 5.5 to 6.5. Viscosity: Spindle T-E @ 40 rpm = 12,400 to 12,600 cP.